MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.

Information provided by SAX Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Viscosity Test 150 cm³/g1.50 dl/gH2SO4; ISO 307
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 118 MPa17100 psi5 mm/min; ISO 527-1
Elongation at Break 2.5 %2.5 %5 mm/min; ISO 527-1
Tensile Modulus 8.30 GPa1200 ksi1 mm/min; ISO 527-1
Flexural Strength 180 MPa26100 psi2 mm/min; ISO 178
Flexural Modulus 6.70 GPa972 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  6.50 kJ/m²
@Temperature -30.0 °C
3.09 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  39.0 kJ/m²
@Temperature -30.0 °C
18.6 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1U
 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched  4.60 J/cm²
@Temperature -30.0 °C
21.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 5.70 J/cm²
@Temperature 23.0 °C
27.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 239 °C462 °F80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 248 °C478 °FB/120; ISO 306
Flammability, UL94 V-0V-0
Glow Wire Ignition Temperature 750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 295 °C536 - 563 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C
@Time 7200 - 21600 sec
176 °F
@Time 2.00 - 6.00 hour
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3HG3 PA66 (Dry)
BASF Ultramid® A3HG3 PA66 (Conditioned)
Avient Edgetek® NN-20GF/000 Nylon 6/6, 20% Glass Fiber Reinforced
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled
Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced

PSAXP952 / 150901

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.