MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Ceramics HR-3M Dense Aluminum Oxide Support Rod
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Together they form a strong skeleton which fixes and supports the hot face insulation throughout a furnace. High alumina content plus excellent strength and creep resistance allow them to provide useful support in furnaces operating to 1800°C, (3292°F).

Type HR-3 Support Rods are 1/4in. diameter, dense ceramic rods for use in conjunction with Hanger Rods Type HR-2 or as individual supports imbedded within an insulation panel. They are available in two different compositions. Type HR-3M Support Rods are high density tubes of mullite composition. This 80% Al2O3 / 20% SiO2 body provides exceptional strength in most applications. HR-3A Support Rods are 99.8% aluminum oxide for use in applications where chemical attack resistance is of concern.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
 
Component Elements PropertiesOriginal ValueComments
Al2O3 80 %
SiO2 20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Ceramics AS-CEM Alumina-Silica Cement
Sandvik Osprey HTN 6 Brazing Powder
Sandvik Kanthal Super HT Molybdenum disilicide
Sandvik Kanthal Super 1900 Molybdenum disilicide
Morgan Advanced Ceramics Palnicro™ Mac-Palnicro™ 36M-WM Braze Alloy

CZIR911 / 138553

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.