MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives Turbo Fuse Series 110SI Surface Insensitive (5 Viscosity) Rapid Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications. The fast curing qualities make it especially desirable in high speed industrial production. Turbo Fuse is ideal for use in applications that require good "wicking" characteristics and/or in close fitting applications. Because of TurboFuse 110SI Series low viscosity, it works especially well in close fitting applications such as metal to metal bonding, and rubber to rubber such as "O" ring repair/manufacture.

Part Numbers for this data: 04-110SI, 10-110SI, 15-110SI, 20-110SI, 25-110SI, 30-110SI, 35-110SI

Soluble in Acetone, MEK, Amide, Methylene Chloride

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 123-31-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccLiquid State
Viscosity 2.0 - 5.0 cPLiquid State
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 65Cured State
Shear Strength 2500 psiTensile, (Cured State)
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.33
@Frequency 1e+6 Hz
Cured State
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °FCured State
Softening Point 300 °FCured State
Minimum Service Temperature, Air -65.0 °FCured State
Flash Point 170 - 200 °FLiquid State (Tagliabue closed cup)
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthLiquid State
 
Descriptive Properties
AppearanceClear liquidLiquid State
 Clear-HardCured State
Base compound (Resin)Surface Insensitive Ethyl CyanoacrylateLiquid State
Gap Fill0.002"Cured State
Material Set Up Time<3 secRubber to Rubber
 3-10 secPolycarbonate to Polycarbonate
 3-5 secPhenolic to Phenolic
 3-5 secAluminum to Aluminum
 5-15 secSteel to Steel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML013 / 135167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.