MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Magnesium AZ63A-T6, Sand Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Sand Casting is ASTM B 80; SAE J465. Good room temperature strength, ductility, and toughness. Commonly used for parts in commercial and military structural applications requiring moderate strength and good ductility and toughness. Not typically used anymore - largely superseded by AZ91.

Key Words: UNS M11630; Elektron AZG; Mg; Old SAE 50; AMS 4420; AMS 4422; AMS 4424; ASTM B 80; SAE J465 (Ingot UNS M11631)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 73500 kg load, 10 mm ball
Hardness, Knoop 96Estimated from Brinell
Hardness, Rockwell E 73
Hardness, Vickers 83Estimated from Brinell
Tensile Strength, Ultimate 275 MPa
 55.0 MPa
@Temperature 315 °C,
Time 601 sec
tested at elevated temperature
 110 MPa
@Temperature 205 °C,
Time 3.60e+6 sec
tested at elevated temperature
 165 MPa
@Temperature 150 °C,
Time 601 sec
tested at elevated temperature
Tensile Strength, Yield 130 MPa
@Strain 0.2 %
Elongation at Break 5.0 %in 50 mm
Tensile Modulus 45.0 GPa
Compressive Yield Strength 130 MPaat 0.2% offset
Ultimate Bearing Strength 415 MPa
Bearing Yield Strength 360 MPa
Poissons Ratio 0.35
Fatigue Strength 76.0 MPa
@# of Cycles 5.00e+8
R.R. Moore Test
 76.0 - 103 MPa
@# of Cycles 1.00e+8
Rotating Beam, R=-1
 82.0 - 110 MPa
@# of Cycles 1.00e+7
Rotating Beam, R=-1
 103 - 124 MPa
@# of Cycles 1.00e+6
Rotating Beam, R=-1
 117 - 138 MPa
@# of Cycles 100000
Rotating Beam, R=-1
 151 - 172 MPa
@# of Cycles 1.00e+7
Direct stress, R=0.25
 158 - 172 MPa
@# of Cycles 1.00e+6
Direct stress, R=0.25
 172 - 207 MPa
@# of Cycles 100000
Direct stress, R=0.25
Machinability 100 %Relative Rating, 100=Best
Shear Modulus 17.0 GPa
Shear Strength 145 MPa
Charpy Impact 1.50 JV-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000118 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 373 J/g
CTE, linear 26.1 µm/m-°C
@Temperature 0.000 - 100 °C
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
Estimated from similar Mg alloys
Specific Heat Capacity 1.05 J/g-°C
Thermal Conductivity 61.0 W/m-K
Melting Point >= 360 °CIncipient Melting
Solidus 455 °C
Liquidus 610 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 705 - 845 °CSand Casting
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.3 - 6.7 %
Copper, Cu <= 0.25 %
Magnesium, Mg 91 %As Remainder
Manganese, Mn >= 0.15 %
Nickel, Ni <= 0.010 %
Silicon, Si <= 0.30 %
Zinc, Zn 2.5 - 3.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium AZ63A-F, Sand Cast
Overview of materials for Magnesium Alloy
Magnesium Alloys, General
Magnesium AM20-F, Die Cast
Magnesium AM60A-F, Die Cast

MMAZ63 / 12323

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.