Description: Low viscosity, condensation crosslinking silicone casting compound Key Features - Low viscosity
- High hardness (Shore A)
- Convincing by reproduction exactness and drawing exactness of the molding
- Molding of simple geometric parts
Application: Molding of simple geometric partsInformation provided by CHT Group |