MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical NBR 8300 High Acrylonitrile Polymer  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: NBR 8300 is a copolymer of butadiene-acrylonitrile and the powdered nitrile elastomer manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 8300 has excellent compatibility with up to 100 parts of PVC resin, its plasticizers, fillers, heat/UV stabilizers and pigments. Within a PVC matrix, NBR 8300 adds the oil and fuel resistance to PVC compound and also it can improve the impact resistance of PVC. NBR 8300/PVC blend acts like a TPEs and substitutes for vulcanized rubber and TPU in many applications due to its excellent fuel and grease resistance.

Applications: NBR 8300 is recommended to use in overflow tubing, vacuum tubing, grommet seals, cable sleeves, gaiters, guard bellows, fuel hoses and seals. In other applications, it is used as modifier for ABS crash pads and also as binder for brake linings.

CAS No: 9003-18-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
Volatiles 0.50 %
Mooney Viscosity 49
@Temperature 100 °C
ML 1+4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 59Forming
 65Fuel Resistance
 69Heat Resistance
 54
@Temperature 25.0 °C,
Time 259000 sec
Fluid Aging ASTM Fuel D
 70
@Treatment Temp. 121 °C,
Time 605000 sec
Circulating Oven Aging
Tensile Strength at Break 11.0 MPaFuel Resistance
 11.7 MPaHeat Resistance
 12.1 MPaForming
 8.04 MPa
@Temperature 25.0 °C,
Time 259000 sec
Fluid Aging ASTM Fuel D
 11.7 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
Circulating Oven Aging
Elongation at Break 460 %Forming
 480 %Heat Resistance
 500 %Fuel Resistance
 500 %
@Temperature 25.0 °C,
Time 259000 sec
Fluid Aging, ASTM Fuel D
 484 %
@Treatment Temp. 121 °C,
Time 605000 sec
Circulating Oven Aging
300% Modulus 77.3 kg(f)/cm²
@Strain 300 %
Forming
 
Descriptive Properties
Bound AN Content (%)32
ComponentsAntioxidant(WINGSTAY 29)1 phr, Heat Resistance
 Antioxidant(WINGSTAY 29)1 phr, Fuel Resistance
 CaCO310 phr, Forming
 Carbon Black2 phr, Forming
 Forming Agent(CELOGEN AZ-130)0.5 phr, Forming
 NBR 830043.6 phr, Forming
 NBR 830033 phr, Heat Resistance
 NBR 830043.6 phr, Fuel Resistance
 Plasticizer(DOP)70 phr, Fuel Resistance
 Plasticizer(DOP)90 phr, Forming
 Plasticizer(PARAPLEX G-62)3 phr, Forming
 Plasticizer(PARAPLEX G-62)5 phr, Fuel Resistance
 Plasticizer(PARAPLEX G-62)5 phr, Heat Resistance
 Plasticizer(PLASTHALL P550)75 phr, Heat Resistance
 PVC (K=70)96.4 phr, Forming
 PVC(K=70)97 phr, Heat Resistance
 PVC(K=70)96.4 phr, Fuel Resistance
 Stabilizer(MARK 308)1 phr, Fuel Resistance
 Stabilizer(MARK 308)1 phr, Forming
 Stabilizer(MARK 974-A)0.5 phr, Forming
 Stabilizer(MARK 974-A)1 phr, Heat Resistance
 Stabilizer(MARK 974-A)2 phr, Fuel Resistance
 Stearic Acid2 phr, Heat Resistance
 Stearic Acid0.5 phr, Fuel Resistance
Volume Swell+4.2%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical MB838A Opaque impact modifier
LG Chemical PB1120 PVC
Stir SpA LG 57 AT 1 (PVC)
Nitrogen Tribromide, NBr3
INEOS Styrolution Luran® S Q440 ASA

PLAY742 / 148752

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.