MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ganpati Exim TBBS(NS)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C11 H14 N2 S2

Properties : Its industrial product is milk-white or light yellowish brown powder, Specific gravity : 1.26-1.32. Soluble in benzene, chloroform, carbon disulfide, acetone, methanol, ethanol, but hard in gasoline, insoluble in water, dilute acid and dilute alkali.

Application : NS is a Vulcanization accelerator with delayed action, short cure time, has high anti-scorching quality, processing safety. Widely used in all sorts of rubber products and tires, especially the meridian tires. The product is excellent delayed accelerator with more delayed action and great curing rate and so on.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 - 1.32 g/cc0.0455 - 0.0477 lb/in³
Molecular Weight 238 g/mol238 g/mol
Ash <= 0.40 %<= 0.40 %
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 104 °C>= 219 °F
 
Descriptive Properties
AppearanceLight yellow or orange colour pellet
Content<1.5%Insoluble In methanol
Heating Loss<0.4%
Residue<0.1%150µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI069 / 317353

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.