MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficient of friction, low extractables, dimensional stability, gamma sterilizable, chemical inertness, and biodurability. In addition, they are coupled with easy thermoplastic processability. Hardnesses from 80 Shore A to 75 Shore D are available; property data below is typical for 80A.

Information provided by AdvanSource Biomaterials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength, Ultimate 5100 psiASTM D412
Elongation at Break 550 %ASTM D412
100% Modulus 0.850 ksi
@Strain 100 %
300% Modulus 1.75 ksi
@Strain 300 %
Flexural Modulus 15000 psiASTM D790
Tear Strength 420 pliDie C; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 185 °FASTM D1525
 
Processing PropertiesOriginal ValueComments
Zone 1 380 °F
Zone 2 380 °F
Zone 3 380 °F
Die Temperature 400 °F
Melt Temperature 410 °F
Drying Temperature 165 - 175 °F
Dry Time 3 - 4 hour
Moisture Content <= 0.10 %
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
DSM Biomedical Bionate® II 55D Thermoplastic Polycarbonate Polyurethane (PCU)
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
Titanium Ti-6Al-4V (Grade 5), Annealed
AdvanSource Biomaterials HydroSlip™ C Hydrophilic Polyether Aliphatic Polyurethane

PCARDI07 / 27931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.