MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shanghai Potomer Dimethy-5-Sulfoisophthalate Sodium Salt(SIPM)
Categories: Other Engineering Material

Material Notes: CAS. No. 3965-55-7

Application: SIPM is mainly used in producing Dacron, film, etc., especially in the field of Dacron as the third monomer of cation modified polyester(CDP). SIPM has good affinity function with cation dye stuff because of the CDP fiber containing sulfo group, the dyed fiber is bright and lustrous, having a complete range of color and dying deeply, so this kind of fiber is developing quickly at a broad. The output of modified polyester fiber of Japan and USA amounts to more than 15%. The modified fiber has woolens feeling, it is easily blended with fleece and suitable for materials for making garments.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.60<= 0.60[mg KOH/g]
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.20 %<= 0.20 %
 
Descriptive Properties
Absorbance<0.005%
Color/AppearanceWhite powder without impurity
Content<100 ppmSulfate
 <15 ppmChloride content
 <4 ppmFe
 376-380 mg KOH/gSaponification Value

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM161 / 284607

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.