MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akrochem AKROCHEM® DCP Cross-linking agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Akrochem DCP is an organic dialkyl peroxide chemically identified as dicumyl peroxide. It fines use as a cross-linking agent for many rubber elastomers and plastic materials, such as polyethylene and ethylene vinyl acetate. DCP is noted for its non-blooming characteristic and high reactivity at medium processing and curing temperatures (see half-life times below). SADT (self accelerating decomposition temperature) is 75°C and the safe processing temperature (ts2>20 mins.) is 130°C. Store this peroxide as close to room temperature as possible.

Applications: Akrochem DCP peroxide is used as a catalyst for cross-linking many polymers. Due to DCP’s half life, this peroxide provides a good compromise between scorch safety and cure rate. In addition, this crosslinker is listed in FDA CFR 21: Title “Food and Drugs” part 177.2600, Rubber Articles Intended for Repeated Use. The powder or granular forms provide ease of handling and weighing accuracy. In silicone rubber, only vinyl-containing silicones can be cured.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 205 °C320 - 401 °FCure Temp
 
Descriptive Properties
Appearancegranule
Content0.99Peroxide
Half-Life Thermal Decomposition Data1 hrs134°C
 1 minute172°C
 10 hrs116°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH556 / 315474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.