MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lyanchemicals Tech ESBO
Categories: Other Engineering Material

Material Notes: Epoxidized Soybean Oil: Our production of Epoxidized Soybean Oil are in line with international quality certification, according to the EU REACH laws and regulations on the quality of quality management, professionals quality assurance with advanced production equipment, the production from Lyanchemicals is the highest quality and best managed. This product is used for non-toxic PVC products, transparent products, aggregates, transparent bottle, food, drug packaging materials, PVC medical products, blood transfusion bags, paper paste-like, waterproofing roll goods, plastic film etc. Must be ensure that products can be non-toxic, transparent, good thermal stability of light and extend the service life of products.

Information provided by Lyanchemicals Tech Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.982 - 0.998 g/ccGB/T5526-1985
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.50[mg KOH/g]; GB/T1668-1995
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 280 °CGB/T1671-1988
 
Descriptive Properties
Color<150Pt-Co/APHA, GB/T1664-1995
Epoxide Value>6%GB/T1677-1981
 >6.6%ASTM D1652-04
Heat Loss<0.3%25°C, 2 hrs
Heat Stability>5.7%177°C, 3hr, GB/T1677-1981
 >6.25%177°C, 3hr, ASTM D1652-04
Residual Iodine<3.0 g/100gGB/TT1676-1981

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLYANT016 / 318043

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.