MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crosspolimeri EFRHATAN 188 A Polyurethane-Polyether Flame Retardant
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Efrhatan: is the trade-mark of our modified polyurethane-polyether flame retardant halogen free.

Efrhatan 188 A: is a thermoplastic elastomeric polyurethane HFFR compound polyether base with glossy surface. This compound offer outstanding chemical and hydrolysis resistance. The material exhibit excellent physical-mechanical performances resulting in tubes and sheathings with optimal kink resistance, strength characteristics and flame retardant. Good processability and excellent extrusion stability. Material to use on the production of cables for electronic devices connection and technical sheathing.

Certify: Guaina/Sheathing FIAT 7,Z8220 T3

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8888ASTM D2240
Tensile Strength 32.0 MPa4640 psiIEC 60811
 38.4 MPa
@Temperature 120 °C,
Time 605000 sec
5570 psi
@Temperature 248 °F,
Time 168 hour
Heat Ageing; IEC 60811
 38.4 MPa
@Temperature 100 °C,
Time 605000 sec
5570 psi
@Temperature 212 °F,
Time 168 hour
Ageing in IRM 902 oil; UL 1581
Elongation at Break 490 %490 %IEC 60811
 588 %
@Temperature 100 °C,
Time 605000 sec
588 %
@Temperature 212 °F,
Time 168 hour
Ageing in IRM 902 oil; UL 1581
 637 %
@Temperature 120 °C,
Time 605000 sec
637 %
@Temperature 248 °F,
Time 168 hour
Heat Ageing; IEC 60811
Tear Strength 60.0 kN/m342 pliambient; DIN 53515
Abrasion 5050[mm³]; DIN 53516
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Zone 1 155 °C311 °F
Zone 2 165 °C329 °F
Zone 3 185 °C365 °F
Zone 4 190 °C374 °F
Die Temperature 215 - 225 °C419 - 437 °F
Melt Temperature <= 200 °C<= 392 °F
Head Temperature 190 °C374 °F
Dry Time  3.00 hour
@Temperature 90.0 °C
3.00 hour
@Temperature 194 °F
 6.00 hour
@Temperature 105 °C
6.00 hour
@Temperature 221 °F
 
Descriptive Properties
Cold Flex-40°CISO 458
Exercise temperature-41-125°C
Saponification Resistance<200 Mg KOH/gHD 22,10S1
Thermal stability>80 min200°C, ISO R 182/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS020 / 294104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.