MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Go Yen Chemical Goyenchem-DEEP High Effective Organic Phosphate Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No.78-38-6

Goyenchem-DEEP is a new type and high effective organic phosphate flame retardant which is made by GYC Group. By comparison with traditional TCPP, the flame retarded effect of Goyenchem-DEPP is higher than 1.5~2 times. This product can be applied to rigid foamed polyurethane, epoxy resin and various foaming system. Moreover, the grade has now already used and replaced traditional TCPP by many suppliers. Goyenchem-DEEP is also a kind of thinner, with low viscosity and free-halogen, good chemical stability in polyether polyol and double isocyanate component system, can be soluble in water and other organic solvents such as alcohol, ether, benzene, etc.

Intro: Goyenchem-DEEP is a new type and high effective organic phosphate flame retardant which is made by GYC Group. By comparison with traditional TCPP, the flame retarded effect of Goyenchem-DEPP is higher than 1.5~2 times. This product can be applied to rigid foamed polyurethane, epoxy resin and various foaming system. Moreover, the grade has now already used and replaced traditional TCPP by many suppliers. Goyenchem-DEEP is also a kind of thinner, with low viscosity and free-halogen, good chemical stability in polyether polyol and double isocyanate component system, can be soluble in water and other organic solvents such as alcohol, ether, benzene, etc.

Advantages:

  • High effective thinner
  • Good compatibility
  • Excellent durability
  • Chemical stability
  • Halogen-free
  • Odorless, pollution-free, will not bring toxic gas when in the flame retarded processing
  • Good flame retarded performance, the effect is better than TCPP (1.5~2 times)
  • Soluble in water and other solvents such as alcohol, ether, benzene, etc.
Applications:
  • Various resin: epoxy resin, polymer resin
  • Rigid foamed polyurethane
  • Polyethylene, ABS
  • Various foaming system
  • Special coating, paint and ink
  • Composite materials: wood, aerospace materials, etc.
  • Other high value flame retarded application

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 - 1.03 g/cc0.0368 - 0.0372 lb/inĀ³
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 1.0<= 1.0mgKOH/g
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.412 - 1.4181.412 - 1.418
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
AppearanceTransparent liquid
Assay>96.5%
Color=50Hazen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN183 / 266491

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.