MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Armeen DMCD Cocoalkyldimethylamines
Categories: Other Engineering Material

Material Notes: Distilled dimethyl, cocoalkylamine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.789 g/cc
@Temperature 100 °C
0.0285 lb/in³
@Temperature 212 °F
 0.793 g/cc
@Temperature 77.0 °C
0.0286 lb/in³
@Temperature 171 °F
Viscosity  38.2 cP
@Temperature 45.0 °C
38.2 cP
@Temperature 113 °F
 42.2 cP
@Temperature 35.0 °C
42.2 cP
@Temperature 95.0 °F
 46.2 cP
@Temperature 25.0 °C
46.2 cP
@Temperature 77.0 °F
Vapor Pressure  <= 0.000133322 bar
@Temperature 25.0 °C
<= 0.0999998 torr
@Temperature 77.0 °F
 0.000660 bar
@Temperature 60.0 °C
0.495 torr
@Temperature 140 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point -14.0 °C6.80 °F
Boiling Point 60.0 - 172 °C
@Pressure 0.0000666612 MPa
140 - 342 °F
@Pressure 0.00966587 psi
Pour Point -12.0 °C10.4 °F
Flash Point >= 149 °C>= 300 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amine number234-250 mg KOH/g
AppearanceLiquid
Color= 50 Apha
Content=1%Primary + Secondary Amine
 =95%Tertiary Amine
 224-240 g/eqNeutralization equivalent
Equivalent mass235 g/eq
HLB9.4Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY197 / 285720

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.