MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Albis Plastics Polycarbonate PC 221 20/05 E Clear Unfilled  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Amorphous Polycarbonate (PC)

Characteristics: General Purpose, Crystal Clear, High Flow, Good Mold Release

Applications: Parts with Thin Walls, Complex Geometry and/or High Flow Length

Processing: Injection Molding (Melt Temperature: 535-565°F, Mold Temperature: 150-220°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 57.2 MPaASTM D638
Tensile Strength, Yield 60.7 MPaASTM D638
Elongation at Break 120 %ASTM D638
Flexural Modulus 2.21 GPaASTM D790
Izod Impact, Notched 8.01 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 123 °CASTM D648
Flammability, UL94 V-2
@Thickness 3.17 mm
Albis Internal Test
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Melt Temperature 279 - 296 °CInjection
Mold Temperature 66.0 - 104 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) Altech® Eco ECO 2030/219 GF30 IM PA6, Conditioned
Mocom (ALBIS) Alcom® AWL 10/3 WT1308-05LB ABS
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Albis Plastics PC/ABS 35A HF Unfilled
ABW Polymers ABS 510 B PC/ABS Alloy, Black

PZA1B56 / 21743

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.