MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unifrax Fiberfrax® Fibermax Bulk Mullite High-Temperature Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These fibers can be classified into the following general categories:

  • High-Index Fibers
  • High-Temperature Fibers
  • Large-Diameter Fibers
  • Milled Fibers

Unifrax manufactures two high-temperature specialty fibers for use in applications beyond recommended operating temperatures of 2300°F (1260°C). Bulk 8000 is made from high-purity alumina, zirconia, and silica raw materials. This chemistry, along with the unique manufacturing process, provides a fiber which can withstand continuous operating temperatures up to 2450°F (1345°C). Fibermax® Bulk Fiber is a high-temperatuer, polycrystalline mullite fiber. Fibermax fiber can withstand continuous operating temperatures up to 2800°F (1540°C) and is virtually shot free. Fibermax fibers can be blended with regular alumina-silicate Fiberfrax fibers to increase the thermal stability of the blended product beyond that of high-purity bulk fiber.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.00 g/cc3.00 g/cc
 
Thermal PropertiesMetricEnglishComments
Melting Point 1870 °C3400 °F
Maximum Service Temperature, Air 1540 °C2800 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 72 - 75 %72 - 75 %
SiO2 25 - 28 %25 - 28 %
 
Descriptive Properties
ColorWhite
Fiber Index (%)95+
Temperature Grade (°C)1650

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Sikor® S Cordierite
Anderman Ceramics EM60 Mullite
Ceradyne Thermo-Sil® Castable TG Fused Silica
Michelman® FiberMax® 105B Strength enhancing fiber treatment
Versalis SINKRAL G320 ABS

CUNIF074 / 97846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.