MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay MTM® 70
Categories: Polymer; Thermoset

Material Notes: Description: MTM70 is a toughened, variable cure temperature prepreg matrix formulated for the manufacture of structural components operating at elevated service temperatures. After 135°C (275°F) standard cure cycle. MTMT70 provides excellent mechanical performance for components operating at up to 140°C (284°F). After post-cure to 180°C (356°F), MTMT70 will operate at higher temperatures without significant loss of toughness.

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage life at -18°C (0°F)
  • Initial cure temperatures between 85°C and 180°C (185°F to 356°F)
  • Tg steps ahead of cure temperature
  • Good mechanical performance with intermediate and high modulus fibers
  • Variable cure temperature capability
  • Excellent retention of mechanical properties at elevated temperatures
Note 1: Cure cycle: 1.5 hrs at 135°C (275°F), 6.2 bar (90 psi)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³Cured resin, 1.5 hrs at 135°C + 2 hr at 180°C
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 197 MPa28600 psiT800 140-54%, After Impact, Post-cure: 2 hrs at 180°C, Note 1; SRM 2R-94
 220 MPa31900 psiT800 140-54%, After Impact, Note 1; SRM 2R-94
 1481 MPa214800 psiT800 140-54%, 0°, Note 1; ASTM D3410
 1535 MPa222600 psiT1000 140-54%, 0°, Note 1; ASTM D3410
Shear Strength 96.5 MPa14000 psiT1000 140-54%, 0°, Interlaminar, Note 1; ASTM D2344
 103 MPa15000 psiT800 140-54%, 0°, Interlaminar, Note 1; ASTM D2344
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 140 °C284 °F
Glass Transition Temp, Tg 145 °C293 °FDMA E' onset Tg, 1.5 hrs at 135°C
 190 °C374 °FDMA E' onset Tg, 1.5 hrs at 135°C + 2 hrs at 180°C
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC AFLAS® 150L TFE/P Fluoroelastomers
Dow VORAFORCE™ TW 103/TW 120 Epoxy for Composite Systems
Dow SiLK™ I 130 Semiconductor Dielectric Resin
Dow Appeel® 22D843 Ethylene Acrylate
Dow Appeel® 20D784 Ethylene Acrylate

PCYTED181 / 180483

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.