MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen EP540V Polypropylene, Impact Modified; Molded/Extruded
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP540V is a polypropylene impact copolymer, with very high melt flow, low warpage, low odor, and good stiffness-impact balance. Typical applications are component of compounds for molding automotive interior and exterior parts like door panels and bumper fascia, direct injection molding of multimedia packaging like DVD cases, and injection molding of general house wares and thin wall containers. Applications: Bumpers, Exterior Automotive Applications, House wares, Interior Automotive Applications, Multi Media Packaging, Opaque Containers

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 110 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 24.0 MPaASTM D638
Elongation at Yield 4.0 %ASTM D638
Flexural Modulus 1600 MPaASTM D790
Izod Impact, Notched 30.0 J/m
@Temperature -20.0 °C
ASTM D256
 40.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Moplen HP500W Polypropylene
LyondellBasell Moplen EP440G Polypropylene, Impact Modified; Molded/Extruded
Silon Tabond 5008 Adhesive Resin
ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene
ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene

PEQT8954 / 220588

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.