MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

EOS StainlessSteel CX DMSL on EOS M 290
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel

Material Notes: EOS StainlessSteel CX is a tooling grade steel characterized by having a good corrosion resistance combined with high strength and hardness. Parts built from EOS StainlessSteel CX can be machined, shot-peened and polished in as manufactured or heat treated state.

Main Characteristics:

  • Stainless steel with excellent corrosion resistance combined with high strength and hardness
  • The parts are easily machinable and offer excellent polishability
  • The parts offer excellent wear and fatigue resistance
Typical Applications:
  • Chlorinated seawater handling equipment
  • Pulp and paper manufacturing devices
  • Chemical handling equipment

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.69 g/cc0.278 lb/in³ISO 3369
Particle Size 20 - 65 µm20 - 65 µm
Thickness 30.0 microns1.18 milLayer Thickness
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5050ISO 6508
Tensile Strength 1720 MPa249000 psiHorizontal, Heat Treated; ISO 6892-1
 1740 MPa252000 psiVertical, Heat Treated; ISO 6892-1
Tensile Strength, Yield 1650 MPa239000 psiHorizontal, Heat Treated; ISO 6892-1
 1670 MPa242000 psiVertical, Heat Treated; ISO 6892-1
Elongation at Break 6.0 %6.0 %Vertical, Heat Treated; ISO 6892-1
 7.0 %7.0 %Horizontal, Heat Treated; ISO 6892-1
Fatigue Strength 695 MPa
@# of Cycles 1.00e+7
101000 psi
@# of Cycles 1.00e+7
ASTM E466
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.1 µm/m-°C
@Temperature 25.0 - 100 °C
6.17 µin/in-°F
@Temperature 77.0 - 212 °F
ASTM E228
 11.6 µm/m-°C
@Temperature 25.0 - 200 °C
6.44 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM E228
 11.9 µm/m-°C
@Temperature 25.0 - 300 °C
6.61 µin/in-°F
@Temperature 77.0 - 572 °F
ASTM E228
 12.0 µm/m-°C
@Temperature 25.0 - 400 °C
6.67 µin/in-°F
@Temperature 77.0 - 752 °F
ASTM E228
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.2 - 2.0 %1.2 - 2.0 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 11 - 13 %11 - 13 %
Manganese, Mn <= 0.40 %<= 0.40 %
Molybdenum, Mo 1.1 - 1.7 %1.1 - 1.7 %
Nickel, Ni 8.4 - 10 %8.4 - 10 %
Silicon, Si <= 0.40 %<= 0.40 %
 
Descriptive Properties
Surface roughness7.5Ra, Horizontal surface
 9Sa, Horizontal surface
Volume rate3.2 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS949 / 280609

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.