MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Townsend Chemicals RE-POL® 98028 Polyester Polyols – Cast Urethanes
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Known for its use in the production of polyurethane coatings and general polyurethane production, Townsend Chemicals specialize in saturated, high molecular weight hydroxyl terminated polyester polyol for use as intermediates in the production of polyurethanes. Polyester polyols are perfect for creating both rigid and flexible polyurethanes for products such as PU foam and polyurethane coatings. Available in a wide range of physical forms and molecular weights

Applications:

  • Rigid foams
  • Flexible foams
  • Castable elastomers eg. printing rollers
  • Surface and fabric coatings
  • Microcellular shoe systems
  • Thermoplastic PU
  • Moisture cured PU
  • Inks
  • Industrial coating

Information provided by Townsend Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1500 cP1500 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.500.50[mg KOH/g]
 
Descriptive Properties
Equivalent Weight390
Hydroxyl Value145 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTOWNS026 / 306765

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.