MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel; Air-Hardening Steel

Material Notes: Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microstructure. Airdi 150 (D2) has been widely used for many years in cold work applications requiring very high wear resistance. It is machinable in the annealed condition and, like other air-hardening tool steels, exhibits minimal distortion on hardening.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.695 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 221 - 225Annealed
Hardness, Rockwell C 60 - 62
Modulus of Elasticity 207 GPa
Charpy Impact 28.0 JAustenitizing Temperature- 1010°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µm/m-°C
@Temperature 20.0 - 95.0 °C
 11.3 µm/m-°C
@Temperature 20.0 - 205 °C
 12.6 µm/m-°C
@Temperature 20.0 - 540 °C
Thermal Conductivity 20.9 W/m-K
@Temperature 95.0 °C
 24.2 W/m-K
@Temperature 315 °C
 25.6 W/m-K
@Temperature 540 °C
Shrinkage -0.0250 %
@Treatment Temp. 1010 °C
Hardening
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.55 %
Chromium, Cr 11.5 %
Iron, Fe 85.25 %As Remainder
Molybdenum, Mo 0.90 %
Vanadium, V 0.80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm AISI D2 Cold Work Tool Steel
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
Carpenter No. 610® High Carbon, High Chrome Tool Steel (Air-Wear) (AISI D2)
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
AISI Type A2 Tool Steel

NCRUC016 / 16009

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.