MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kohesi Bond KB 1031 AT-2LO Two component, cryogenically serviceable flexibilized epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Superior thermal conductivity
  • Tremendous flexibility and elongation
  • Cryogenic service
  • Soaring peel strength
  • Exceptional electrical insulation properties
  • Capable of passing NASA low outgassing
Kohesi Bond KB 1031 AT-2LO is a two component, highly flexibilized epoxy system suitable for bonding, sealing, potting and encapsulation. It has a favorable 1:3 (Part A: Part B) mix ratio by weight. It offers stellar thermal conductivity and is capable of passing NASA low outgassing test, unlike most flexible epoxies. This epoxy system readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. KB 1031 AT-2LO can withstand severe thermal shocks and cycling even at cryogenic temperatures. It offers an extensive service temperature range of 4K (-269.15°C) to +120°C. It fosters outstanding physical strength properties and yet consolidates high peel strength and elongation. KB 1031 AT-2LO adheres well to a wide variety of substrates including metals, ceramics, most plastics and glass. It offers excellent chemical resistance to a variety of fuels, oils and water. Part A has a gray color and Part B has an off-white color. Owing to its excellent performance and vacuum compatibility KB 1031 AT-2LO is widely used in electronics and related industries.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 36000 - 85000 cPPart A
 300000 - 810000 cPPart B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35 - 40
Tensile Strength >= 3200 psi
Elongation at Break >= 25 %
Adhesive Bond Strength >= 900 psiTensile Lap Shear, Al/Al
Peel Strength >= 18.0 pliT-peel Strength, Al/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -269 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 90.0 °C
Option 2
 3.00 - 5.00 hour
@Temperature 70.0 - 90.0 °C
Optimum Cure: overnight at 23°C plus 3 - 5 hours at 70°C - 90°C
 48.0 - 72.0 hour
@Temperature 23.0 °C
Option 1
Working Life >= 65.0 min100 g of mixed epoxy
 
Descriptive Properties
Mixing Ratio1:3 by weightPart A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOHESI900 / 249079

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.