MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Danquinsa DANCOLL® 245-20 Poly adduct
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLL® 245-20 is a poly adduct containing hydroxyl groups with a low solvent content which is used for the production of adhesives for polyethylene bags and film laminations. This product serves as a Tackifier and tack improver in PE bag adhesive solutions. As a Tackifier, DANCOLL® 245-20 is also added to harder PUR adhesives.

Application: For its application in the PE-bag bonding, DANCOLL® 245-20 was developed in a very soft and elastic version. A long-lasting self tack of the product provides additional safety in long processing cycles. DANCOLL® 245-20 is processed in a two-component way, mainly in connection with our poly isocyanate DANCURE® 246-13. As a modification component, DANCOLL® 245-20 is added to PUR-adhesives which require a long open time and a high tack. Depending on the total formulation, approx. 8 to 15 % of a cross linking agent is added to DANCURE® 246-13.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³DIN 51.757
Solids Content 73 - 76 %73 - 76 %DIN 53.189
Brookfield Viscosity 8000 - 20000 cP8000 - 20000 cPRVT
 
Thermal PropertiesMetricEnglishComments
Flash Point -3.00 °C26.6 °FDIN 51.755
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspectclear and transparent liquid
SolventEthyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ020 / 294440

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.