Selar® RB 300 barrier resin is a pellet blend of nylon homolymer and a proprietary adhesive for nylon and polyethylene. Selar® RB 300 is a food grade resin designed for use in blends with polyethylene (HDPE, LDPE, LLDPE) in extrusion blowmolding of articles made with DuPont proprietary Laminar Technology. The DuPont Laminar Technology has also been used for other processes such as sheet extrusion and tube extrusion. Information provided by DuPont Packaging Polymers. |
Polyamide; DuPont Packaging Polymers |