MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Traid Villarroya TRAIDAMID® G black Nylon 6, Cast
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes:
  • High strength
  • Resistant to many greases, oils and fuels
  • High toughness
  • Good slide and wear resistance
  • Good wear properties
Industry Applications:
  • Heavy duty industry
  • Conveyor technology
  • Textile industry
  • Engine manufacturing
  • Mechanical engineering

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Water Absorption  0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
DIN EN ISO 62
 0.40 %
@Time 346000 sec
0.40 %
@Time 96.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa21800 psiISO 2039-1
Tensile Strength 70.0 MPa10200 psi50 mm/min; DIN EN ISO 527-2
Tensile Strength, Yield 68.0 MPa9860 psi50 mm/min; DIN EN ISO 527-2
Elongation at Break 50 %50 %50 mm/min; DIN EN ISO 527-2
Elongation at Yield 4.0 %4.0 %50 mm/min; DIN EN ISO 527-2
Modulus of Elasticity 3.10 GPa450 ksi1 mm/min; DIN EN ISO 527-2
Flexural Strength 95.0 MPa
@Load 1.02 kg
13800 psi
@Load 2.25 lb
2 mm/min; DIN EN ISO 178
Flexural Modulus 2.90 GPa
@Load 1.02 kg
421 ksi
@Load 2.25 lb
2 mm/min; DIN EN ISO 178
Compressive Strength  21.0 MPa
@Strain 1 %,
Load 1.02 kg
3050 psi
@Strain 1 %,
Load 2.25 lb
5 mm/min; EN ISO 604
 37.0 MPa
@Strain 2 %,
Load 1.02 kg
5370 psi
@Strain 2 %,
Load 2.25 lb
5 mm/min; EN ISO 604
Compressive Modulus 2.70 GPa
@Load 1.02 kg
392 ksi
@Load 2.25 lb
5 mm/min; EN ISO 604
Charpy Impact Unnotched NBNBMax. 7,5j; DIN EN ISO 179-1EU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²Max. 7,5j; DIN EN ISO 179-1EU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmDIN IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear  130 µm/m-°C
@Temperature 23.0 - 60.0 °C
72.2 µin/in-°F
@Temperature 73.4 - 140 °F
DIN EN ISO 11359-1;2
 130 µm/m-°C
@Temperature 23.0 - 100 °C
72.2 µin/in-°F
@Temperature 73.4 - 212 °F
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°FISO 22007-4:2008
Thermal Conductivity 0.370 W/m-K2.57 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 216 °C421 °FDIN 53765
Maximum Service Temperature, Air 100 °C212 °FLong term
 170 °C338 °FShort term
Glass Transition Temp, Tg 42.0 °C108 °FDIN 53765
Flammability, UL94 HBHBDIN IEC 60995-11-10
 
Descriptive Properties
ColorBlack opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAID903 / 318864

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.