MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® 2850FT/11 Two-Component Thermally Conductive Encapsulant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Provides excellent heat dissipation and thermal shock resistance as well as protection from moisture and chemical agents. Typical applications include sensors, transformers, transducers, switches, and other small devices.
  • Mix Ratio by weight = 100:4.5
  • Excellent Chemical Resistance
  • Filled
  • High temperature
Cure Type: Heat Bonding Type: Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.29 g/ccMixed
 2.40 g/ccPart A, Loctite Stycast 2850FT
Water Absorption 0.050 %
@Time 86400 sec
Immersion
Viscosity 48 cPPart B, Loctite CAT 11
 64000 cPMixed
Brookfield Viscosity 250000 cPPart A, Loctite Stycast 2850FT; Spindle 7, Speed 10 rpm
 250000 cPPart A, Loctite Stycast 2850FT, Small Sample Adapter; Spindle 14, speed 3 rpm
Linear Mold Shrinkage 0.0020 cm/cm
Outgassing - Total Mass Loss 0.020 %NASA Method, Sample cured 4 hours @ 80ºC; CVCM
 0.29 %NASA Method, Sample cured 4 hours @ 80ºC; TML
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 96
Flexural Strength 117 MPa
Compressive Strength 193 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Dielectric Constant 5.36
@Frequency 1e+6 Hz
Dielectric Strength 15.0 kV/mm
Dissipation Factor 0.043
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.2 µm/m-°CAlpha 1
 97.9 µm/m-°CAlpha 2
Thermal Conductivity 1.28 W/m-K
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -55.0 °C
Glass Transition Temp, Tg 115 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 1.00 hour
@Temperature 120 °C
Option 3. Post cure of 2 to 4 hours at the highest expected use temperature is recommended.
 2.00 - 4.00 hour
@Temperature 100 °C
Option 2. Post cure of 2 to 4 hours at the highest expected use temperature is recommended.
 8.00 - 16.0 hour
@Temperature 80.0 °C
Option 1. Post cure 2 to 4 hours at the highest expected use temperature is recommended.
Working Life 240 min
@Temperature 25.0 °C
100 g
Shelf Life 12.0 MonthPart A, Loctite Stycast 2850FT
 
Descriptive Properties
AppearanceBlackPart A, Loctite Stycast 2850FT
Mix Ratio, by Volume100 : 9.5Material : Catalyst
Mix Ratio, by Weight100 : 4.5Material : Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 2850FT-FR/11 Two-Component Epoxy Flame Retardant Encapsulant
Henkel Hysol EA 9396/C-2 Paste Adhesive System
Henkel Hysol EA 9396.6MD Paste Adhesive System
Henkel Hysol EA 9396 Paste Adhesive System
Henkel Hysol EA 9309.3NA Paste Adhesive System

PEMERS36 / 35728

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.