MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 Transmission Oil 90
Categories: Fluid; Lubricant

Material Notes: Conoco® Transmission Oil 90 is an SAE 90 mineral oil gear lubricant recommended for use in manual transmissions, transfer cases and rear axle assemblies of automotive, farm and off-highway equipment where the manufacturer specifies an API GL-1 gear oil. It also may be used in light-duty industrial applications where a non-compounded, ISO VG 150 or AGMA 4 mineral oil is specified. Transmission Oil 90 has good film strength and rust inhibition to protect gears, bearings and synchronizers. It also has good oxidation resistance to help minimize deposit formation, and good resistance to foaming.

Applications:

  • Heavy-duty, multiple-speed manual transmissions and transfer cases in trucks and buses where the manufacturer specifies an API GL-1, SAE 90 gear oil
  • Lightly loaded enclosed industrial gear drives where the OEM specifies a R&O type, AGMA 4 gear oil
  • General-purpose lubrication in applications that require a non-compounded, ISO VG 150 mineral oil
Transmission Oil 90 meets the requirements of:
  • API Service GL-1
Features/Benefits:
  • Good film strength for wear protection
  • Good oxidation resistance
  • Protects against rust and corrosion
  • Good foam resistance

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Conoco® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.882 g/cc0.882 g/cc
API Gravity 29.7 °29.7 °
Viscosity Measurement 9797Viscosity Index
Saybolt Viscosity at 100°F 830 SUS830 SUS
Saybolt Viscosity at 210°F 81 SUS81 SUS
Kinematic Viscosity at 40°C (104°F) 149 cSt149 cSt
 158 cSt158 cSt
Kinematic Viscosity at 100°C (212°F) 15.3 cSt15.3 cSt
ASTM Color 2.52.5
 2.52.5ASTM D1500
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Flash Point 277 °C530 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Transmission Oil SAE 90 ISO Grade 150, AGMA Grade 4
Evonik POLYVEST® 110 Liquid
Evonik Polyoil 110 Polybutadiene
ConocoPhillips Hydroclear Diamond Class® Turbine Oil 68
ChevronTexaco Superla® 50 White Oil

WCON024 / 75061

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.