MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Uniplex FRP-45 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex FRP-45 is a liquid flame retardant that imparts efficient flame retardance to a large number of polymers (e.g. flexible PVC, TPO and elastomers) due to its high bromine content. It offers a very low volatility combined with a superior thermal and color stability.

Chemical name: Di-2-ethylhexyl tetra bromo phthalate

CAS - No: 26040-51-7

Applications: Uniplex FRP-45 is especially recommended for applications like cable & wires or conveyer belts. It is also suitable for adhesives, coatings, films and coated fabrics.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.541 g/cc0.05567 lb/inĀ³
Water Absorption <= 0.10 %<= 0.10 %
Viscosity 1595 cP1595 cP
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 3.0<= 3.0
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br 45.0 %45.0 %
 
Descriptive Properties
Appearanceclear amber liquid
Assay>95%
Content<0.1%Tetra bromo phthalic anhydride
 <0.3%2-Ethylhexanol
Specifications<0.05 mEq/100gAcidity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Uniplex FRP-45I Plastic Additive
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4"
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8"
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8"
Lanxess Uniplex FRP-64 Plastic Additive

PLANY9118 / 209509

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.