MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® B3 GF 50 S1 PA, Cold-Impact Resistant, 50% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilization for the engine compartment or very good UV- resistance for the out door area. However, calcium chloride is critical with regard to PA6.6. In combination with anti-freeze containing window cleaning fluid, an ugly white film is emerging on the surface. Main applications are window cleaning fluid valves, head light cleaning units, wiper end caps, bezels etc. in the front area of the automobile.

Information from Akro-Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 185 MPa
Charpy Impact, Notched 30.0 kJ/m²

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 6 GF 45 Polyamide 6, 45% Glass Fiber
Latrobe Lescalloy® 4340 VAC-ARC ; 3.5" round High Strength Alloy Steel
RTP Company RTP PA6 50 GF BLK Nylon 6 (PA), Value Product - Glass Fiber - Heat Stabilized
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® UT-18 VAC-ARC ; 6 in. round High Strength Alloy Steel

PAKRO091 / 126871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.