Dielectric is suitable for use as an insulation layer when printed and fired on to stainless steel. The thermal coefficient of expansion of this product has been matched to that of stainless steel. It is compatible with a range of high temperature conductors available from the GEM product range. It is suitable for printing directly on to stainless steel. Screen Printing Equipment: semi-automatic, automatic Screen Types: stainless steel, polyester, mesh 156-325 tpi Substrate: stainless steelInformation provided by Gwent Electronic Materials Ltd. |