MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® SB1006 Thermoplastic Elastomer for RF Interference Control
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description:
  • Made with a flexible thermoplastic elastomer giving it rubber-like properties.
  • Designed for good absorption over wide frequency range.
  • Can be optimized for higher frequencies, such as24 and 77 GHz.
  • Excellent elongation, flexibility, and UV resistance.
  • Reflection loss performance will vary depending upon sheet thickness requested.
  • Standard sheet size: 24” x 24” (60.96 cm x 60.96 cm) Other sheet sizes are available upon request.
  • Can be water-jet or die cut.
  • Halogen free, RoHS and REACH compliant.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 77.077.0ASTM D2240
Tensile Strength 11.3 MPa1640 psiASTM D638
Elongation at Break 902 %902 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 2.622e+8 ohm>= 2.622e+8 ohmASTM D257
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9578 / 322732

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.