MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Kolon CI900 Matte Electrically Insulating Film  (discontinued **)
Categories: Polymer; Film

Material Notes: CI Series have outstanding mechanical properties, high durability, adhesive strength and electrical insulation. Used for Solar Cell Modules, Back Sheets, Front Sheet,s Motor Insulation, Cable wrapping, Insulation Tape, Labels, FPCB Boards, Carriers, Membrane Switches.

Information provided by Kolon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.0 - 188 microns0.472 - 7.40 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD  230 %
@Thickness 0.125 mm
230 %
@Thickness 0.00492 in
ASTM D882
 240 %
@Thickness 0.190 mm
240 %
@Thickness 0.00748 in
ASTM D882
 240 %
@Thickness 0.250 mm
240 %
@Thickness 0.00984 in
ASTM D882
Film Elongation at Break, TD  130 %
@Thickness 0.125 mm
130 %
@Thickness 0.00492 in
ASTM D882
 170 %
@Thickness 0.250 mm
170 %
@Thickness 0.00984 in
ASTM D882
 200 %
@Thickness 0.190 mm
200 %
@Thickness 0.00748 in
ASTM D882
Coefficient of Friction, Dynamic  0.30
@Thickness 0.125 mm
0.30
@Thickness 0.00492 in
ASTM D1894
 0.30
@Thickness 0.190 mm
0.30
@Thickness 0.00748 in
ASTM D1894
 0.38
@Thickness 0.250 mm
0.38
@Thickness 0.00984 in
ASTM D1894
Coefficient of Friction, Static  0.30
@Thickness 0.125 mm
0.30
@Thickness 0.00492 in
ASTM D1894
 0.30
@Thickness 0.190 mm
0.30
@Thickness 0.00748 in
ASTM D1894
 0.35
@Thickness 0.250 mm
0.35
@Thickness 0.00984 in
ASTM D1894
Film Tensile Strength at Break, MD  176 MPa
@Thickness 0.125 mm
25500 psi
@Thickness 0.00492 in
ASTM D882
 176 MPa
@Thickness 0.190 mm
25500 psi
@Thickness 0.00748 in
ASTM D882
 176 MPa
@Thickness 0.250 mm
25500 psi
@Thickness 0.00984 in
ASTM D882
Film Tensile Strength at Break, TD  176 MPa
@Thickness 0.190 mm
25500 psi
@Thickness 0.00748 in
ASTM D882
 176 MPa
@Thickness 0.250 mm
25500 psi
@Thickness 0.00984 in
ASTM D882
 196 MPa
@Thickness 0.125 mm
28400 psi
@Thickness 0.00492 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD  1.0 %
@Thickness 0.125 mm
1.0 %
@Thickness 0.00492 in
Heat Shrinkage; ASTM D2305
 1.0 %
@Thickness 0.190 mm
1.0 %
@Thickness 0.00748 in
Heat Shrinkage; ASTM D2305
 1.0 %
@Thickness 0.250 mm
1.0 %
@Thickness 0.00984 in
Heat Shrinkage; ASTM D2305
Shrinkage, TD  0.50 %
@Thickness 0.125 mm
0.50 %
@Thickness 0.00492 in
Heat Shrinkage; ASTM D2305
 0.50 %
@Thickness 0.190 mm
0.50 %
@Thickness 0.00748 in
Heat Shrinkage; ASTM D2305
 0.50 %
@Thickness 0.250 mm
0.50 %
@Thickness 0.00984 in
Heat Shrinkage; ASTM D2305
 
Optical PropertiesMetricEnglishComments
Haze  1.4 %
@Thickness 0.125 mm
1.4 %
@Thickness 0.00492 in
ASTM D1003
 2.4 %
@Thickness 0.190 mm
2.4 %
@Thickness 0.00748 in
ASTM D1003
 4.0 %
@Thickness 0.250 mm
4.0 %
@Thickness 0.00984 in
ASTM D1003
Gloss 20 - 40 %20 - 40 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOKZ821 / 185364

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.