MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical MU620 ABS, Low Deformation  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Feature: Extrusion Molding, Low Deformation

Application: Mock-Up

CAS No. 9003-56-9

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Maximum Moisture Content 0.010Extrusion Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength, Yield 380 kg(f)/cm²
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Break 25 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Yield >= 5.0 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Flexural Yield Strength 700 kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Flexural Modulus 26000 kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Izod Impact, Notched 32.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 36.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 92.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Zone 1 180 - 210 °CExtrusion Molding
Zone 2 190 - 230 °CExtrusion Molding
Zone 3 200 - 250 °CExtrusion Molding
Zone 4 200 - 250 °CExtrusion Molding
Adapter Temperature 200 - 250 °CExtrusion Molding
Die Temperature 200 - 250 °CExtrusion Molding
Melt Temperature 200 - 250 °CExtrusion Molding
Roll Temperature 60.0 - 90.0 °CBottom, Extrusion
 70.0 - 90.0 °CMiddle, Extrusion
 70.0 - 100 °CTop, Extrusion
Drying Temperature 70.0 - 80.0 °CExtrusion Molding
Dry Time 3.00 - 4.00 hourExtrusion Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
LG Chemical SG175 ABS, Super Surface Gloss
LG Chemical PT270 ABS
LG Chemical MA201 ABS, Low Gloss
LG Chemical HI100K ABS, High Impact

PLAY032 / 148040

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.