MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix, Unidirectional Prepreg Laminate (M36/32%/135/HTA)
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Tenax HTA fiber

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 365 MPaOpen Hole Tension, Hot/Wet
 384 MPa
@Temperature 23.0 °C
Open Hole Tension
 2143 MPa
@Temperature 23.0 °C
Tensile Modulus 140 GPa
@Temperature 23.0 °C
Compressive Yield Strength 204 MPaCompression After Impact, 30J
 205 MPaCompression After Impact, 40J
 243 MPaCompression After Impact, 20J
 251 MPaOpen Hole Compression, Hot/Wet
 278 MPaCompression After Impact, 10J
 273 MPa
@Temperature 23.0 °C
Open Hole Compression
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber

PHEXC178 / 98649

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.