MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for PVC, Wire and Cable Grade
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.880 - 2.06 g/cc0.0318 - 0.0744 lb/in³Average value: 1.38 g/cc Grade Count:1287
Moisture Absorption at Equilibrium 0.300 - 0.570 %0.300 - 0.570 %Average value: 0.414 % Grade Count:7
Loss On Ignition 23.0 - 54.0 %23.0 - 54.0 %Average value: 28.2 % Grade Count:46
Viscosity 0.950 - 2.37 cP0.950 - 2.37 cPAverage value: 1.64 cP Grade Count:3
 473000 - 473000 cP
@Temperature 177 - 177 °C
473000 - 473000 cP
@Temperature 351 - 351 °F
Average value: 473000 cP Grade Count:1
 473000 - 473000 cP
@Frequency 1000 - 1000 Hz
473000 - 473000 cP
@Frequency 1000 - 1000 Hz
Average value: 473000 cP Grade Count:1
Linear Mold Shrinkage 0.0100 - 0.0180 cm/cm0.0100 - 0.0180 in/inAverage value: 0.0120 cm/cm Grade Count:33
Melt Flow 0.200 - 30.0 g/10 min0.200 - 30.0 g/10 minAverage value: 5.92 g/10 min Grade Count:79
ASTM Color -3.17 - 93.1-3.17 - 93.1Average value: 18.8 Grade Count:11
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30.0 - 99.030.0 - 99.0Average value: 80.9 Grade Count:1101
Hardness, Shore D 33.0 - 77.033.0 - 77.0Average value: 49.5 Grade Count:144
Hardness, Shore C 65.0 - 92.065.0 - 92.0Average value: 78.5 Grade Count:77
Tensile Strength, Ultimate 1.11 - 35.0 MPa161 - 5080 psiAverage value: 15.4 MPa Grade Count:896
Tensile Strength, Yield 2.07 - 53.1 MPa300 - 7700 psiAverage value: 14.8 MPa Grade Count:439
Elongation at Break 0.000 - 920 %0.000 - 920 %Average value: 302 % Grade Count:1156
Elongation at Yield 128 - 450 %128 - 450 %Average value: 303 % Grade Count:180
Modulus of Elasticity 0.00600 - 1.12 GPa0.870 - 163 ksiAverage value: 0.0377 GPa Grade Count:41
Flexural Modulus 0.0752 - 1.30 GPa10.9 - 188 ksiAverage value: 0.524 GPa Grade Count:3
Tear Strength 22.0 - 104 kN/m126 - 593 pliAverage value: 48.6 kN/m Grade Count:9
Graves Tear Strength 52.0 - 73.5 kN/m297 - 419 pliAverage value: 66.0 kN/m Grade Count:3
Compression Set 26.0 - 71.0 %26.0 - 71.0 %Average value: 40.2 % Grade Count:14
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.10 - 5.60e+15 ohm-cm2.10 - 5.60e+15 ohm-cmAverage value: 4.87e+14 ohm-cm Grade Count:270
 2.60e+9 - 9.60e+16 ohm-cm
@Temperature 50.0 - 50.0 °C
2.60e+9 - 9.60e+16 ohm-cm
@Temperature 122 - 122 °F
Average value: 1.10e+16 ohm-cm Grade Count:17
Insulation Resistivity 747 - 747 Megaohm/1000 m
@Temperature 15.6 - 15.6 °C
2450 - 2450 Megaohm/1000 ft
@Temperature 60.0 - 60.0 °F
Average value: 747 Megaohm/1000 m Grade Count:1
Dielectric Constant 2.10 - 7.042.10 - 7.04Average value: 3.98 Grade Count:73
Dielectric Strength 21.0 - 39.4 kV/mm533 - 1000 kV/inAverage value: 30.1 kV/mm Grade Count:22
Dissipation Factor 0.000100 - 0.1900.000100 - 0.190Average value: 0.0670 Grade Count:58
 0.0580 - 0.0900
@Temperature 30.0 - 30.0 °C
0.0580 - 0.0900
@Temperature 86.0 - 86.0 °F
Average value: 0.0740 Grade Count:2
 0.0580 - 0.0900
@Frequency 1000 - 1000 Hz
0.0580 - 0.0900
@Frequency 1000 - 1000 Hz
Average value: 0.0740 Grade Count:2
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:26
Hot Wire Ignition, HWI 15.0 - 120 sec15.0 - 120 secAverage value: 75.3 sec Grade Count:26
High Amp Arc Ignition, HAI 30.0 - 120 arcs30.0 - 120 arcsAverage value: 87.7 arcs Grade Count:25
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 23.9 - 205 °C75.0 - 401 °FAverage value: 87.9 °C Grade Count:453
Minimum Service Temperature, Air -65.0 - -20.0 °C-85.0 - -4.00 °FAverage value: -39.8 °C Grade Count:19
Brittleness Temperature -100 - 15.0 °C-148 - 59.0 °FAverage value: -29.7 °C Grade Count:794
UL RTI, Electrical 50.0 - 90.0 °C122 - 194 °FAverage value: 82.1 °C Grade Count:34
UL RTI, Mechanical with Impact 50.0 - 90.0 °C122 - 194 °FAverage value: 55.3 °C Grade Count:14
UL RTI, Mechanical without Impact 50.0 - 90.0 °C122 - 194 °FAverage value: 80.3 °C Grade Count:31
Flammability, UL94 HB - V-0HB - V-0Grade Count:76
Oxygen Index 12.0 - 62.0 %12.0 - 62.0 %Average value: 29.4 % Grade Count:744
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80.0 - 90.0 %80.0 - 90.0 %Average value: 89.0 % Grade Count:20
 
Processing PropertiesMetricEnglishComments
Processing Temperature 157 - 191 °C315 - 375 °FAverage value: 174 °C Grade Count:46
Nozzle Temperature 188 - 249 °C370 - 480 °FAverage value: 205 °C Grade Count:34
Die Temperature 150 - 249 °C302 - 480 °FAverage value: 202 °C Grade Count:37
Melt Temperature 110 - 390 °C230 - 734 °FAverage value: 184 °C Grade Count:538
Head Temperature 130 - 165 °C266 - 329 °FAverage value: 146 °C Grade Count:3
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FAverage value: 44.2 °C Grade Count:34
Roll Temperature 21.1 - 48.9 °C70.0 - 120 °FAverage value: 35.0 °C Grade Count:4
Drying Temperature 82.2 °C180 °FAverage value: 82.2 °C Grade Count:4
Injection Pressure 0.0689 - 6.89 MPa10.0 - 1000 psiAverage value: 3.67 MPa Grade Count:34
Cushion 0.381 - 2.54 cm0.150 - 1.00 inAverage value: 1.46 cm Grade Count:30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Extruded
Overview of materials for PVC, Flexible Grade
Overview of materials for PVC, Molded
Overview of materials for Chlorinated PVC (CPVC)
Overview of materials for PVC, Rigid Grade

O5643 / 78522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.