MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 20-2180 Polyurethane Potting & Encapsulating Resins
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This series of polyurethane systems is engineered for electronic potting, encapsulating, and casting applications. They are low in viscosity, low in toxicity and available in the popular TriggerBond® dual barrel cartridge dispensing system. These elastomeric systems are suitable for a variety of electronic insulating applications. The durometers range from an enterable gel to Shore A 80.

Green: The base Natural Oil Polyol (NOP) used in these systems is obtained directly from a plant source without chemical modifications. Using renewable resources, such as NOP’s, will reduce the demand on non-renewable fossil fuels and reduce the overall production of carbon dioxide.

Features:

  • Green
  • Low Viscosity
  • Available in TriggerBond
  • Low Durometer
  • Moisture Resistant
  • Convenient Mix Ratios
  • Low Shrinkage & Exotherm
Benefits:
  • Reduce demand on non-renewable fossil fuels
  • Quick self leveling around components
  • Easy to use packaging
  • Low stress on components & vibration resistant
  • Can be used in wet environments
  • Easy to process by hand or with meter mix
  • Less stress to components during cure

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccPolyol Resin
 1.15 g/cc1.15 g/ccIsocyanate
Viscosity 1500 cP1500 cPIsocyanate
 1700 cP1700 cPMixed
 2200 cP2200 cPPolyol Resin
Storage Temperature 21.0 - 29.0 °C69.8 - 84.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080
Elongation at Break 220 %220 %
Tear Strength 14.0 kN/m80.0 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
Dielectric Strength 25.6 kV/mm650 kV/in
Dissipation Factor 0.017
@Frequency 1000 Hz
0.017
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 210 µm/m-°C117 µin/in-°F
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 20.0 min20.0 min
 
Descriptive Properties
ColorBlack
Mix Ratio1:2Iso:Polyol, by volume
 60:100Iso:Polyol, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX012 / 316689

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.