MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil HD 6909.65 High Density Polyethylene Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stiffness or enable down-gauging. This material offers excellent performance in structural foam articles.

Availability: Latin America, North America and South America

Additive:

  • Antioxidant: Yes
  • UV Stabilizer: Yes
Applications:
  • Cases
  • Crates
  • Hot Fill Packaging Pails
  • Materials Handling Articles
  • Pallets
  • Structural Foam Articles
  • Totes Bins

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.965 g/cc0.0349 lb/in³ExxonMobil method
ESCR 10% Igepal® 3.0 hour3.0 hourF50; ASTM D1963B
Melt Flow 8.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 3.03 MPa440 psiASTM D638
Tensile Strength, Yield 30.3 MPa4400 psiASTM D638
Flexural Modulus 1.59 GPa
@Strain 2 %
230 ksi
@Strain 2 %
Secant; ASTM D790B
Flexural Modulus, 1% Secant 1860 MPa270000 psiASTM D790B
Izod Impact, Notched 0.475 J/cm
@Temperature -40.0 °C
0.890 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 135 °C<= 275 °FPeak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C189 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.3 °C119 °FASTM D648B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9708 HDPE Injection Molding Resin
Dow HDPE 12450N High Density Polyethylene
Dow 722 Linear Low Density Polyethylene (LDPE)
Chevron Phillips Marlex® H516 Polyethylene; HDPE
Westlake EC1390AA Low Density Polyethylene

PEX99303 / 175539

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.