MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon M6080UV HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Alathon M6080UV is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include cases, tote bins, crates and trays. M6080UV contains a UV stabilizer for outdoor applications.

Availability: North America

Application: Crates; Pallets/Trays/Tote Bins

Market: Rigid Packaging

Processing Method: Injection Molding

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.593 - 0.625 g/ccASTM D1895
Density 0.960 g/ccASTM D1505
Melt Flow 7.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 21.8 cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D <= 70.0ASTM D2240
Tensile Strength at Break 15.9 MPaASTM D638
Tensile Strength, Yield 29.3 MPaASTM D638
Elongation at Break 380 %ASTM D638
Elongation at Yield 11.0 %ASTM D638
Flexural Modulus 1070 MPa2% Secant; ASTM D790
 1310 MPa1% Secant; ASTM D790
 1410 MPaASTM D790
1% Secant Modulus 848 MPaASTM D638
Izod Impact, Notched 75.0 J/mASTM D256
Izod Impact, Unnotched NB
@Temperature -18.0 °C
ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Melting Point 132.7 °CASTM D3418
Crystallization Temperature 115.9 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CASTM D648
Vicat Softening Point 129 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9041 / 323969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.