MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives LokRelease 200 Aqueous Mold Release
Categories: Fluid

Material Notes: LORD® LokRelease™ 200 aqueous mold release is designed for use with molded elastomers, including EPDM, natural rubber, nitrile and neoprene. This water-based mold release provides a nontransferable and non-interfering anti-stick coating for fast, easy part removal from molds.

Features: provides quick, easy part release; produces low build-up, allowing more production time between mold cleanings; improves molding efficiency in many processes including injection, compression and transfer molding. reduces defects caused by sticking; nontransferable, eliminating post-finishing problems. water-based coating is engineered to prevent rust and corrosion in steel molds.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.999 g/cc0.0361 lb/in³
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature <=27.0 °C
12.0 Month
@Temperature <=80.6 °F
from manufacture date in original, unopened container
 
Descriptive Properties
AppearanceColorless to White Liquid
Dispersing MediumWater

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9100 / 232489

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.