MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Bicor® 110 ASB-X OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. ASB-X is good for heavy dump VFFS applications (e.g., bulk tortillas) due to its excellent hot tack and seal strength. This film is suitable as an unsupported web or in a lamination. It can be surface printed, reverse printed or used unprinted.

Availability: Latin America, North America and South America

Key Features:

  • Outstanding optical properties
  • Robust machinability
  • Low and consistent COF
  • Excellent flavor and aroma barrier
  • Excellent heat seal strength and hot tack
  • Very good moisture barrier
  • Good Oxygen barrier
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
  • Gas Barrier
  • In Lamination Lap sealable
  • Moisture Barrier
  • Oxygen Barrier
  • PVdC Coated
Applications:
  • Biscuits/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Sugar
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pre-made Bags - Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Out Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 5.10 g/m²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Oxygen Transmission Rate 70.0 cc/m²/day23°C, 0% RH; ExxonMobil Method
Thickness 1.10 milNominal; ExxonMobil Method
Coating Weight 16.2 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.23ExxonMobil Method
Film Tensile Strength at Break, MD 20000 psiExxonMobil Method
Film Tensile Strength at Break, TD 35000 psiExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 4.5 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 3.5 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 1.1 %ExxonMobil Method
Gloss 98 %45º; ExxonMobil Method
 
Descriptive Properties
Crimp Seal MST190°FPVdC/PVdC
Crimp Seal Strength650 g/inPVdC/PVdC, 260°F, 20psi, 0.8 sec
Yield26600 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global 110 Polypropylene
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade

PEXB378 / 37683

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.