MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller Cyberbond SM 77 Adhesive
Categories: Polymer; Adhesive

Material Notes: Profile: Sealant and retainer: High strength, high viscosity, thixotropic, high temperature resistant. Anaerobic sealant and retainer for dynamic loaded parts like bearings, shafts etc. with high temperature resistance.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/cc
Viscosity  1000 - 6000 cP
@Shear Rate 160 1/s
1000 - 6000 cP
@Shear Rate 160 1/s
cone-plate
 4000 - 10000 cP
@Shear Rate 0.500 1/s
4000 - 10000 cP
@Shear Rate 0.500 1/s
cone-plate
Storage Temperature 8.00 - 21.0 °C46.4 - 69.8 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 26.0 - 46.0 MPa
@Time 86400 sec
3770 - 6670 psi
@Time 24.0 hour
Steel pin/collar specimen
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.167 - 0.500 min0.00278 - 0.00833 hourSet time, M10 brass bolt/nut
 1440 min24.0 hourFull Cure
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesive strength10-20 NmBrass
 14-24 NmStainless steel V2A
 18-30 NmGalvanized steel
 30-40 NmSteel
Base compoundDimethacrylate
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL051 / 316842

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.