MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmodur® IL 1451 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Desmodur IL 1451 is an aromatic polyisocyanate based on toluene diisocyanate (TDI). It is used as a hardener component for fast drying, two-component polyurethane coatings.

Properties / Applications: The two-component polyurethane systems formulated with Desmodur IL 1451 are characterized by their very rapid initial drying and early sandability, making them ideal for the industrial coating of wood and furniture. An NCO/OH ratio of approx. 0.5 - 0.7 is recommended as a function of the reactivity and hardness of the polyol. With an NCO/OH ratio of 1:1, the Desmodur IL 1451 must be combined with Desmodur L. In this case, the optimal ratio of the Desmodur L / IL 1451 is a function of polyol hardness and the required drying time. The low viscosity and high reactivity of the Desmodur IL 1451 enables the formulation of clear and colored coatings with high solids contents. These can be applied quickly and only a few coats are required. As with any product, use of Desmodur IL 1451 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Volatiles 49 - 53 %
Viscosity 175 - 325 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point 26.0 °C
 
Descriptive Properties
Color<2Iodine
Content<0.5%Monomeric
 7.2-7.6%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmodur® IL BA Polyurethane
Covestro Desmodur® L 67 BA Polyurethane
Covestro Desmodur® I Polyurethane
Covestro Desmodur® IL 1351 Polyurethane
Covestro Desmodur® H Polyurethane

PCOVEST0355 / 202138

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.