MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right balance between: -Adhesion onto non-wovens – Flexibility after coating – Barrier for fluids and gases LD 259 can also be used as a general extrusion and co-extrusion coating grade, showing – Easy processability – Good neck-in/draw down balance – Excellent heat sealability Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Coextrusion Coating
  • Demanding Heat Seals
  • Document Plastification
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • High Speed, Thin Weight Coatings
  • Industrial Packaging
  • Non-woven coating
  • Photographic Paper
  • Thermal Lamination

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.915 g/cc0.0331 lb/in³ExxonMobil method
Melt Flow 12 g/10 min12 g/10 minASTM D1238
Neck In  4.32 cm
@Temperature 315 °C
1.70 in
@Temperature 599 °F
656 ft/min, Constant output at 35 rpm; ExxonMobil Method
 4.57 cm
@Temperature 315 °C
1.80 in
@Temperature 599 °F
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
Drawdown 9.17 m/s
@Temperature 315 °C
1810 ft/min
@Temperature 599 °F
Constant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 104 °C<= 219 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin
ExxonMobil LDPE LD 251 Low Density Polyethylene Resin (European Grade)
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin
Eastman 1390P Polyethylene

PEX99279 / 175515

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.