MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Sandvik Cuprothal 15 Resistance Wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: NIKROTHAL 40 is used as electric heating element material in domestic appliances and other electric heating equipment at operating temperatures up to 1100°C (2010°F). It has good ductility after use, good corrosion resistance except in sulphur containing atmospheres and certain controlled atmospheres and excellent weldability.

Typical applications for NIKROTHAL 40 are night-storage heaters, convection heaters, heavy duty rheostats and fan heaters. NIKROTHAL 40 is also used in heating cables and rope heaters in defrosting and de-icing elements, electric blankets and pads, car seats, baseboard heaters, floor heaters, resistors, etc.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 300 MPa
@Thickness 1.00 mm
43500 psi
@Thickness 0.0394 in
Tensile Strength, Yield 130 MPa
@Strain 0.2 %,
Thickness 1.00 mm
18900 psi
@Strain 0.2 %,
Thickness 0.0394 in
Elongation at Break 30 %
@Thickness 1.00 mm
30 %
@Thickness 0.0394 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000150 ohm-cm0.0000150 ohm-cm
 0.0000150 ohm-cm
@Temperature 20.0 °C
0.0000150 ohm-cm
@Temperature 68.0 °F
 0.0000155 ohm-cm
@Temperature 100 °C
0.0000155 ohm-cm
@Temperature 212 °F
 0.0000160 ohm-cm
@Temperature 200 °C
0.0000160 ohm-cm
@Temperature 392 °F
 0.0000166 ohm-cm
@Temperature 300 °C
0.0000166 ohm-cm
@Temperature 572 °F
 0.00001725 ohm-cm
@Temperature 400 °C
0.00001725 ohm-cm
@Temperature 752 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.89 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.380 J/g-°C
@Temperature 20.0 °C
0.0908 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 60.0 W/m-K
@Temperature 20.0 °C
416 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1100 °C2010 °F
Maximum Service Temperature, Air 400 °C752 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 89 %89 %
Nickel, Ni 11 %11 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Cuprothal 30 Resistance Wire
Oxygen-free Copper (OF), UNS C10200, OS050 temper, wire
Sandvik Cuprothal 5 Resistance Wire
Sandvik Cuprothal 49 and 49TC Resistance Wire
Oxygen-free Electronic Copper (OFE), UNS C10100, H08 Temper, wire

NSANDV085 / 18979

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.