MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3XZG5 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant; Nylon 66, Impact Grade

Material Notes: Product Description: Ultramid® A3XZG5 is an impact-modified, 25% glass fiber reinforced injection molding PA66 grade with improved flame retardance. Flame retardant based on red phosphorus. Applications; Typical applications include components with high stiffness, dimensional stability and enhanced impact strength such as electrical switches.

Availability: Asia Pacific; Europe; North America

Filler/Reinforcement: Glass Fiber, 25% Filler by Weight

Additive: Flame Retardant(Red phosphorus); Impact Modifier

Features: Flame Retardant; Good Impact Resistance; High Dimensional Stability; High Stiffness; Impact Modified: Oil Resistant

Use: Electrical Parts; Switches

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Automotive Specifications: FMVSS 302

Forms: Pellets

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Maximum Moisture Content 0.0500.050
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.3 MPa10200 psiISO 527-2
Elongation at Break 11 %11 %ISO 527-2
Tensile Modulus 4.50 GPa653 ksiISO 527-1
Charpy Impact Unnotched 10.1 J/cm²48.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 2.94 J/cm²14.0 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 - 300 °C545 - 572 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 3.50 - 12.5 MPa508 - 1810 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2072 / 310765

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.