MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Ceramics AXL Alumina-Silica Insulation
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity and excellent thermal shock resistance. AXL is designed for use to 1260°C (2300°F), AXHTM is useful to 1427°C (2600°F).

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.280 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 20ASTM 02240
Flexural Strength 0.170 MPaParallel to thickness
Compressive Yield Strength 0.0500 MPaat 10% Compression, Parallel to thickness
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.100 W/m-K
@Temperature 400 °C
 0.170 W/m-K
@Temperature 800 °C
 0.220 W/m-K
@Temperature 1100 °C
Maximum Service Temperature, Air 1260 °C
Shrinkage 1.8 %
@Temperature 1000 °C,
Time 86400 sec
Perpendicular to Thickness
 2.5 %
@Temperature 1200 °C,
Time 86400 sec
Perpendicular to Thickness
 
Component Elements PropertiesOriginal ValueComments
Al2O3 38 %
SiO2 62 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Foam
Overview of materials for Silicone Rubber
Overview of materials for Acetal Copolymer, Silicone Filled
Morgan Advanced Ceramics M120F Mac-AS970W Aluminum silicate Ceramic
Goodfellow Leachable Ceramic (Silica, Zircon, Alumina)

CZIR034 / 2842

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.