MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis NAV102 LDPE, post-consumer recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: NAV102 is a translucent low density polyethylene post-consumer recycled (rLDPE) supplied in pellet form for high-end blown film applications. NAV102 is an ideal LDPE used where sustainability and circularity matter. NAV102 is a 100% post-consumer recycleds including a large part of recycled post-consumer plastic waste coming from pre-sorted municipal (household) waste. NAV102 is part of the EuCertPlast certificate according to the European Standard EN 15343:2007 (certificate available upon request). Due to the nature of recyclates, some variation in color can be observed between batches.

Typical characteristics:

  • Translucent
  • Filtration: 100 µm
  • Available in homogenized 24-ton truckloads
Applications:
  • Collation shrink film
  • Shrink film
  • Lamination films for non-food contact primary packaging
  • Non-food contact primary packaging
  • Secondary and tertiary packaging where reasonable optics are needed
  • Transparent bags
  • Industrial packaging
  • Carrier bags/light colors
  • Agriculture films
  • Foam Applications
Note: Minor quantity of BorShape" LLDPE significantly boosts mechanical performances of NAV102 helping convertors, brand owners and retailers meeting their sustainability goals without compromising key mechanical properties for similar packaging performance.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.490 g/ccISO 60
Density 0.925 g/ccISO 1183
Melt Flow 0.850 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 220 %527-3
Film Elongation at Break, TD 255 %527-3
Tensile Modulus 215 MPaMD; ISO 527-3
 255 MPaTD; ISO 527-3
Elmendorf Tear Strength MD 143 gISO 6383-2
Elmendorf Tear Strength TD 479 gISO 6383-2
Dart Drop Test 75.0 gISO 7765-1
Film Tensile Strength at Break, MD 13.0 MPa527-3
Film Tensile Strength at Break, TD 15.0 MPa527-3
 
Optical PropertiesOriginal ValueComments
Haze 35.0 %ASTM D1003
Gloss 30.0 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 160 - 190 °C
Moisture Content <= 0.0500 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9830 / 323187

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.