MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAKEEP® iC4506 R PEEK, 6% barium sulphate
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: VESTAKEEP® iC4506 R is a rod stock based on implantable grade polyether ether ketone resin VESTAKEEP® iC4506 G. It contains 6% barium sulphate to render it X-ray opaque.
Dry properties listed below
Industrial Sector: Medical Devices Processing: Machining
Delivery form: Stock shape (rods and plates)
Optics: Opaque
Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering
Electrical: Insulating
Conformity: Biocompatibility, Medical application
Additives: Mineral fillers
Applications: Medical implants
Special Characteristics: Phosphorus-free, PTFE-free, High impact strength, Semi-crystalline, High viscosity, Self-extinguishing
Features: Low odor, Non-corrosive
Color: Natural color
Additives: Inorganic fillers
Chemical Resistance: Acid resistance, Solvent resistance, Oxidation resistance, Radiation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Water Absorption 0.400 %0.400 %Sim to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 109 MPa15800 psiISO 527
Tensile Strength, Yield 109 MPa15800 psiISO 527
Elongation at Break 4.60 %4.60 %ISO 527
Elongation at Yield 4.60 %4.60 %ISO 527
Tensile Modulus 4.20 GPa609 ksiISO 527
Flexural Strength 170 MPa24700 psiISO 178
Flexural Modulus 4.20 GPa609 ksiISO 178
Izod Impact, Notched (ISO) 5.40 kJ/m²2.57 ft-lb/in²Type of failure: C; ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Melting Point 340 °C644 °FISO 11357-1/-3
Glass Transition Temp, Tg 145 °C293 °F2nd heating, onset; ISO 11357
 155 °C311 °F2nd heating, midpoint; ISO 11357
 
Processing PropertiesMetricEnglishComments
Recrystallization Temperature 285 °C545 °F20 K/min; ISO 11357
 
Descriptive Properties
ColorNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7870 / 325002

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.