MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Synthos ES-IJ65 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: ES-IJ series is a special kind of polyester-based thermoplastic polyurethane elastomer, which is designed for injection molding products.

Features:

  • Fast molding
  • Good flexibility
  • High transparency and resilience
  • Excellent abrasion resistance
  • Good hand feeling and texture
  • Excellent mechanical properties
Application: Electronics coating, key, wire plug, shoe, handle pedometer, watch band, air bag, water balls, electronics cover, auto part, dust-proof cover, garment accessories, animal tag, sealing gasket, machine part, composite modified, roller, sports equipment part, etc.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 - 1.21 g/cc0.0423 - 0.0437 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 63 - 6763 - 67ASTM D2240
Tensile Strength 15.0 - 25.0 MPa2180 - 3630 psiASTM D412
Elongation at Break 600 - 900 %600 - 900 %ASTM D412
100% Modulus 1.00 - 5.00 MPa145 - 725 psiASTM D412
300% Modulus 2.00 - 8.00 MPa290 - 1160 psiASTM D412
Tear Strength 40.0 - 100 kN/m228 - 571 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg <= -38.0 °C<= -36.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUNDOW161 / 320192

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.