MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation
Categories: Polymer; Thermoplastic

Material Notes: Tygon S3™ E-LFL from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Tygon S3™ line combines the high performance standards customers demand with an eco-friendly tubing design. The new Tygon S3™ E-LFL non-DEHP tubing is our best performing peristaltic pump tubing. Tygon S3™ E-LFL has been tested rigorously to ensure that it meets the same physical standards as the old Tygon® LFL tubing, including 1,000 hours of peristaltic pump tubing life at 0 psi back pressure, low particulate spallation and chemical resistance.

Crystal-clear Tygon S3™ E-LFL tubing is formulated specifically for use in peristaltic pump applications. With its superior flex life characteristics, manufacturing processes can be simplified by reducing production downtime due to pump tubing failure. The excellent wear properties of Tygon S3™ E-Long Flex Life Pump Tubing also lead to a reduction of particulate spallation. This feature limits the risk of sensitive-fluid contamination critical to the pharmaceutical, cosmetic, food and beverage industries.

Non-aging characteristics and broad chemical resistance provide users with versatility in use for a wide variety of applications. Safe and non-toxic Tygon S3™ E-Long Flex Life Pump Tubing can be produced in up to a 6" inside diameter, making it the ideal choice in bulk transfer applications.

Applications

  • Wide range of liquid transfer in labs
  • Production filtration and fermentation
  • Food & beverage and cosmetic processing
  • Biopharmaceutical
  • Surfactant delivery
  • Flavor and vitamin concentrate dispensing
  • Printing ink transfer
  • Highly viscous fluid transfer
  • Drum and tank drainage
  • Shear-sensitive fluid transfer

Features and Benefits

  • Longest flex life of any clear Tygon® tubing -- reduces downtime due to pump failure
  • Extremely low particulate spallation -- reliable for sensitive-fluid applications
  • Broad chemical resistance -- excellent for laboratory applications
  • Can be autoclaved -- suitable for high purity applications
  • Contains no BPA or phthalate

Regulatory Information: Tygon S3™ complies with FDA, NSF, 3-A, USP Class VI, ISO 10993, Japan Food Sanitation Law # 370/1959, REACH, 1935/2004/EC and 10/2011/EC for many foods and beverages. Tygon S3™ tubing products do not contain chemicals listed in California's Prop 65.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Water Absorption 0.20 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 56
@Time 15.0 sec
ASTM D2240
Tensile Strength 1800 psiASTM D412
Tensile Stress at Strain 550 psi
@Strain 100 %
ASTM D412
 950 psi
@Strain 200 %
ASTM D412
Elongation at Break 400 %ASTM D412
Tear Strength 184 pliASTM D1004
Compression Set 68 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
Tensile Set 54 %at 75 % elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Minimum Service Temperature, Air -67.0 °Ftemperature limit for flexibility
Brittleness Temperature -51.0 °FASTM D746
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Clear, but value not quantified
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA Yes
NSF Yes
USP Class VI Yes
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture
Saint-Gobain Tygon® A-60-F Food Process Tubing Formulation
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation

PSTGQ914 / 160410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.